Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
250 words
An improved chemical vapor deposition method of producing a fluorine-doped tin oxide coating which has a minimum and constant sheet resistance under different process conditions, comprising: (a) forming a liquid coating composition which includes an organic fluorine dopant and an organotin compound, said composition comprising: (1) 1-30 wt./ of an organic fluorine dopant wherein at least one fluorine atom is located alpha or beta to a functional group wherein carbon is bonded to oxygen selected from carboxylic acid, anhydride, ester, alcohol, ketone, acid halide, or ether; and (2) 70-99 wt./ of an organotin compound, which is an alkyltin trichloride, a dialkyltin dichloride, an alkyldichlorotin acetate, a dialkylchlorotin diacetate, or an ester tin trichloride; or tin tetrachloride; (b) vaporizing said liquid coating composition into a wet carrier gas to form a vapor mixture of carrier gas, water, organic fluorine dopant and organotin compound; and (c) decomposing said vapor mixture on a substrate to form said coating, characterized in that: the vapor concentrations of said components are such that a parameter M, defined as: where (AIR) is the concentration of the carrier gas, in moles, (H20) is the concentration of water in the carrier gas, in moles, (OFD) is the concentration of organic fluorine dopant in the carrier gas, in moles, and (0) is the concentration of organotin compound in the carrier gas, in moles, has a value of less than 50,000, thereby to produce a fluorine-doped tin oxide coating having a minimum and constant sheet resistance for said values of M.
Claim 2
Dependent Claim
250 words
An improved chemical vapor deposition method of producing a fluorine-doped tin oxide coating which has a minimum and constant sheet resistance under different process conditions, comprising: (a) forming a liquid coating composition which includes an organic fluorine dopant and an organotin compound, said composition comprising: (1) 1-30 wt./ of an organic fluorine dopant wherein at least one fluorine atom is located alpha or beta to a functional group wherein carbon is bonded to oxygen selected from carboxylic acid, anhydride, ester, alcohol, ketone, acid halide, or ether; and (2) 70-99 wt./ of an organotin compound, which is an alkyltin trichloride, a dialkyltin dichloride, an alkyldichlorotin acetate, a dialkylchlorotin diacetate, or an ester tin trichloride; or tin tetrachloride; (b) vaporizing said liquid coating composition into a wet carrier gas to form a vapor mixture of carrier gas, water, organic fluorine dopant and organotin compound; and (c) decomposing said vapor mixture on a substrate to form said coating, characterized in that: the vapor concentrations of said components are such that a parameter M, defined as: where (AIR) is the concentration of the carrier gas, in moles, (H20) is the concentration of water in the carrier gas, in moles, (OFD) is the concentration of organic fluorine dopant in the carrier gas, in moles, and (0) is the concentration of organotin compound in the carrier gas, in moles, has a value of less than 50,000, thereby to produce a fluorine-doped tin oxide coating having a minimum and constant sheet resistance for said values of M.
Claim 3
Dependent Claim
18 words
A process according to claim 1 wherein M has a value of 20,000 or less. or claim 2,
Claim 4
Dependent Claim
28 words
A process according to claim 1/in which the sheet resistance of the coating produced thereby is about 25 ohms/sq. at a thickness of about 180-210 nm. any preceding
Claim 5
Dependent Claim
28 words
A process according to/claim in which the liquid coating composition comprises 2-10 wt.X of said organic fluorine dopant, and 90-98% of said organotin compound. claims 1 to 3,
Claim 6
Dependent Claim
21 words
A process according to any of/ wherein said liquid coating composition includes up to 10 wt.% of a polar organic compound.
Claim 7
Dependent Claim
21 words
A process according to any of/ wherein said liquid coating composition includes up to 10 wt.% of a polar organic compound.
Claim 8
Dependent Claim
31 words
A process according to claim 5 wherein said composition includes 2-10 wt.% of said organic fluorine dopant, 80-97 wt.% of said organotin compound, and 1-10 wt.% of said polar organic compound.
Claim 9
Dependent Claim
21 words
claim 5 or 7. A process according to/claim 6 wherein said polar organic compound is acetic anhydride, ethyl acetate or methylisobutylketone.
Claim 10
Dependent Claim
13 words
any preceding 8. A process according to/claim wherein said vaporization temperature is 100-400°C.
Claim 11
Dependent Claim
17 words
A process according to any preding claim wherein said deposition temperature is above 400° and below 700°C.
Claim 12
Dependent Claim
11 words
A process according to claim 1 wherein said substrate is glass.
Claim 13
Dependent Claim
20 words
The product of the process of claim 1 having a substantially minimum and constant sheet resistance with increasing deposition temperature.
Claim 14
Dependent Claim
32 words
A process according to any of claims 1 to 10, wherein said organotin compound is monobutyltin trichloride, methyltin trichloride, isobutyltin trichloride, dibutyltin dichloride, di-t-butyltin dichloride, butyldichlorotin acetate, butylchlorotin diacetate, or carbethoxyethyltin trichloride.