Water resistant aluminum particles and coating
Assignee: Silberline Manufacturing Co Inc
•
Filing: 1984-06-26
•
Granted: —
•
Expires: 2004-06-26
Abstract
Abstract Metal particles, e.g. aluminum, are treated with ionic r organic phosphate, being thereby transformed to a state capable of resisting attack from an aqueous medium. The treated particles may be incorporated into a water-borne coating.
Inventors
- 👤 James Earl Williams, Jr.
- 👤 Pamela Louise Claassen
Bibliographic Details
Application Number
—
Jurisdiction
EP
Data Source
google_patents
Last Synchronized
2026-10-29 10:48
CPC Classifications
C; C09; C09D; C09D5/00; C09D5/38; C09C; C09C1/00; C09C1/62; C09C1/64; C09C1/644; C09D17/00; C09D17/004; C09D17/006; C01; C01P; C01P2006/00; C01P2006/12; C01P2006/60; C01P2006/80; Y; Y10; Y10T; Y10T428/00; Y10T428/29; Y10T428/2982; Y10T428/2991
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
199 words
A composition characterized by comprising metal particles which include compound of the formulae of Figures lA, 1B or lC in an effective concentration to retard the reaction of the metal with water, thereby inhibiting the evolution of hydrogen gas, where in said formulae, and where Z is hydrogen or means for neutralizing acid phosphate; and where R is benzo, a halo group, an alkyl group having from 1 to 24 carbon atoms, a cycloalkyl group having from 3 to 20 carbon atoms, an aryl group having from 6 to 40 carbon atoms, a halo substituted aryl group wherein said aryl has from 6 to 40 carbon atoms, an alpha or beta naphthyl, a halo substituted alpha or beta naphthyl, a 3 to 20 carbon atom cycloalkyl substituted alpha or beta naphthyl, an alpha or beta alkyl substituted naphthyl wherein said alkyl has from 1 to 24 carbon atoms, or a heterosubstituent substituted aryl wherein said aryl has from 6 to 40 carbon atoms, and said heterosubstituent consists of CN, N0 2 , COOH, CHO, OH, a pyridinyl, an alpha or beta furyl, or an alpha or beta thienyl, and, if desired, further comprising a compatible liquid and a surfactant.
Claim 2
Dependent Claim
199 words
A composition characterized by comprising metal particles which include compound of the formulae of Figures lA, 1B or lC in an effective concentration to retard the reaction of the metal with water, thereby inhibiting the evolution of hydrogen gas, where in said formulae, and where Z is hydrogen or means for neutralizing acid phosphate; and where R is benzo, a halo group, an alkyl group having from 1 to 24 carbon atoms, a cycloalkyl group having from 3 to 20 carbon atoms, an aryl group having from 6 to 40 carbon atoms, a halo substituted aryl group wherein said aryl has from 6 to 40 carbon atoms, an alpha or beta naphthyl, a halo substituted alpha or beta naphthyl, a 3 to 20 carbon atom cycloalkyl substituted alpha or beta naphthyl, an alpha or beta alkyl substituted naphthyl wherein said alkyl has from 1 to 24 carbon atoms, or a heterosubstituent substituted aryl wherein said aryl has from 6 to 40 carbon atoms, and said heterosubstituent consists of CN, N0 2 , COOH, CHO, OH, a pyridinyl, an alpha or beta furyl, or an alpha or beta thienyl, and, if desired, further comprising a compatible liquid and a surfactant.
Claim 3
Dependent Claim
50 words
A composition as claimed in claim 1, characterized in that it comprises aluminum particles such as flakes which include compound of the formula of Figure 2 in an effective concentration to retard the reaction of the aluminum with water, thereby inhibiting the evolution of hydrogen gas, where, in said formula,
Claim 4
Dependent Claim
20 words
A composition as claimed in claim 2, characterized in that said compound has the formula of Figure 3 or 4.
Claim 5
Dependent Claim
28 words
A composition according to claim 2 or 3, characterized in that said aluminum particles have a surface area of from about 0.05 to about 15 m 2 /gm.
Claim 6
Independent Claim
188 words
A method characterized by comprising contacting metal particles with compound of the formulae of Figures lA, 1B or 1C in an effective concentration to retard the reaction of the metal with water, thereby inhibiting the evolution of hydrogen gas, where in said formulae, and where Z is hydrogen or means for neutralizing acid phosphate; and where R is benzo, a halo group, an alkyl group having from 1 to 24 carbon atoms, a cycloakyl group having from 3 to 20 carbon atoms, an aryl group having from 6 to 40 carbon atoms, a halo substituted aryl group wherein said aryl has from 6 to 40 carbon atoms, an alpha or beta naphthyl, a halo substituted alpha or beta naphthyl, a 3 to 20 carbon atom cycloalkyl substituted alpha or beta naphthyl, an alpha or beta alkyl substituted naphthyl wherein said alkyl has from 1 to 24 carbon atoms, or a heterosubstituent substituted aryl wherein said aryl has from 6 to 40 carbon atoms, and said heterosubstituent consists of CN, N0 2 , COOH, CHO, OH, a pyridinyl, an alpha or beta furyl, or an alpha or beta thienyl.
Claim 7
Independent Claim
188 words
A method characterized by comprising contacting metal particles with compound of the formulae of Figures lA, 1B or 1C in an effective concentration to retard the reaction of the metal with water, thereby inhibiting the evolution of hydrogen gas, where in said formulae, and where Z is hydrogen or means for neutralizing acid phosphate; and where R is benzo, a halo group, an alkyl group having from 1 to 24 carbon atoms, a cycloakyl group having from 3 to 20 carbon atoms, an aryl group having from 6 to 40 carbon atoms, a halo substituted aryl group wherein said aryl has from 6 to 40 carbon atoms, an alpha or beta naphthyl, a halo substituted alpha or beta naphthyl, a 3 to 20 carbon atom cycloalkyl substituted alpha or beta naphthyl, an alpha or beta alkyl substituted naphthyl wherein said alkyl has from 1 to 24 carbon atoms, or a heterosubstituent substituted aryl wherein said aryl has from 6 to 40 carbon atoms, and said heterosubstituent consists of CN, N0 2 , COOH, CHO, OH, a pyridinyl, an alpha or beta furyl, or an alpha or beta thienyl.
Claim 8
Dependent Claim
80 words
A method as claimed in claim 5, characterized in that it comprises contacting (preferably by the cake reduction method) aluminum particles with a compound of the formula of Figure 2, 3 or 4 in an effective concentration to retard the reaction of the aluminum with water, thereby inhibiting the evolution of hydrogen gas, and, if desired, further comprising, following contacting, an aging step, preferably for about 2.weeks, for developing the ability of the aluminum particles to resist reaction with water.
Claim 9
Dependent Claim
23 words
A metal-particle coating, characterized in that the metal particles therein comprise a composition as claimed in any one of claims 1 to 4.
Claim 10
Dependent Claim
15 words
A coating as claimed in claim 7, characterized by said coating being a water-borne coating.
Claim 11
Dependent Claim
18 words
A coating as claimed in claim 7 or 8, characterized in that the metal particles comprise aluminum particles.
Claim 12
Dependent Claim
29 words
A paste characterized by comprising a major amount of a composition as claimed in any one of claims 1 to 4 and a minor amount of a compatible liquid.