← Back to Patent Explorer
EP0125779A2 Expired / Lapsed EP ⏱️ 0.0 years remaining

Skin care formulations comprising a water-in-mineral oil emulsion and siloxane compositions therefor

Assignee: Dow Silicones Corp
•
Filing: 1984-04-06
•
Granted: —
•
Expires: 2004-04-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract

Inventors

  • 👤 Joseph Woodward Keil

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-11-06 01:12
CPC Classifications
A; A61; A61K; A61K8/00; A61K8/18; A61K8/72; A61K8/84; A61K8/89; A61K8/891; A61K8/894; A61K8/02; A61K8/04; A61K8/06; A61K8/064; A61P; A61P17/00; A61Q; A61Q19/00; C; C08; C08G; C08G77/00; C08G77/42; C08G77/46; C08L; C08L83/00; C08L83/10; C08L83/12

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 192 words
An organopolysiloxane having the formula wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula -(OCH 2 CH 2 )p(OCHCH 3 CH 2 )qOR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR' radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p, and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x ≤ 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the organopolysiloxane.
Claim 2
Dependent Claim 192 words
An organopolysiloxane having the formula wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula -(OCH 2 CH 2 )p(OCHCH 3 CH 2 )qOR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR' radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p, and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x ≤ 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the organopolysiloxane.
Claim 3
Dependent Claim 32 words
. An organopolysiloxane according to Claim 1 wherein Z denotes the methyl radical, x has a value of zero and y + z has an average value of from 30 to 70.
Claim 4
Dependent Claim 38 words
An organopolysiloxane according to Claim 2 wherein z has a value of from 1 to 3 and QR' denotes -CH 2 CH 2 CH 2 (OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OH.
Claim 5
Dependent Claim 12 words
An organopolysiloxane according to Claim 3 wherein R denotes the dodecyl radical.
Claim 6
Dependent Claim 35 words
An organopolysiloxane according to Claim 1 wherein x has an average value of from 1 to 100, y + z has an average value of from 30 to 70 and Z denotes the methyl radical.
Claim 7
Dependent Claim 38 words
An organopolysiloxane according to Claim 5 wherein z has a value of from 1 to 3 and QR' denotes -CH 2 CH 2 CH 2 (OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OH.
Claim 8
Dependent Claim 12 words
An organopolysiloxane according to Claim 6 wherein R denotes the dodecyl radical.
Claim 9
Dependent Claim 229 words
A homogeneous composition comprising (A) an organopolysiloxane having the formula Z(CH 3 ) 2 SiO[(CH 3 ) 2 SiO] x [(CH 3 )(R)SiO] y [(CH 3 ) (QR')SiO] y Si(CH 3 ) 2 Z wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula - (OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR'- radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x < 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the'organopolysiloxane, and (B) mineral oil.
Claim 10
Dependent Claim 229 words
A homogeneous composition comprising (A) an organopolysiloxane having the formula Z(CH 3 ) 2 SiO[(CH 3 ) 2 SiO] x [(CH 3 )(R)SiO] y [(CH 3 ) (QR')SiO] y Si(CH 3 ) 2 Z wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula - (OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR'- radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x < 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the'organopolysiloxane, and (B) mineral oil.
Claim 11
Dependent Claim 224 words
An emulsion composition comprising (I) a dispersed phase comprising water and a cosmetically acceptable electrolyte dissolved therein, (II) a cosmetically acceptable continuous phase comprising mineral oil, and (III) an organopolysiloxane having the formula wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula -(OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR'- radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x ≤ 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the organopolysiloxane.
Claim 12
Dependent Claim 224 words
An emulsion composition comprising (I) a dispersed phase comprising water and a cosmetically acceptable electrolyte dissolved therein, (II) a cosmetically acceptable continuous phase comprising mineral oil, and (III) an organopolysiloxane having the formula wherein QR' denotes a polyoxyalkylene radical consisting of a Q portion having the formula -(OCH 2 CH 2 ) p (OCHCH 3 CH 2 ) q OR" and an R' portion linking the Q portion to a silicon atom, R denotes an alkyl radical having from 6 to 16 carbon atoms, R' denotes an alkylene linking radical, R" denotes a hydrogen atom or a lower alkyl radical, Z denotes a monovalent radical selected from the group consisting of hydrocarbon radicals having from 1 to 5 carbon atoms, QR'- radicals and R radicals, there being an average of at least one QR'- radical and an average of at least one R radical per molecule of organopolysiloxane and the average values of x, y, z, p and g being such that p ≥ g, p + g has a value sufficient to provide a radical weight for Q of from 600 to 3500, x ≤ 3y, x + y + z has a value of from 30 to 400 and the total weight of Q radicals in the organopolysiloxane does not exceed a value of 1/3 of the total weight of the organopolysiloxane.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag