← Back to Patent Explorer
EP0106477A2 Expired / Lapsed EP ⏱️ 0.0 years remaining

Process for manufacturing semiconductor devices comprising an electrochemical-etching step

Assignee: AT&T Inc
•
Filing: 1983-09-01
•
Granted: —
•
Expires: 2003-09-01
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A procedure is described for producing semiconductor devices having damage-free surfaces in electrochemically n-type and intrinsic compound semiconductors. The process involves a photoetching procedure including applying a potential to the compound semiconductor while it is in contact with an electrolytic solution and irradiating the surface to be etched with light in a certain energy range. By suitable adjustment in the potential, electrolytic solution composition and light energy, the etch rate is made proportional to the light intensity. By suitable variation in light intensity and light-ray direction, various geometrical features can be made on the surface of the compound semiconductor. For example, a hole with straight sides can be made in the compound semiconductor by use of a light spot and parallel (collimated) light rays. An advantageous application of this process is the fabrication of a photodiode with a hole in the center for use in bidirectional communication systems and to monitor power output for optical communication sources. The advantage of this process is that no damage occurs outside etched hole so that a maximum area of the photodiode remains active for detecting incoming radiation. Another advantage of the process is that etching will stop where the material becomes p-type so that etching can be made to stop automatically at a p/n junction.

Inventors

  • 👤 Stephen Ross Forrest
  • 👤 Paul Albert Kohl
  • 👤 Richard Lawrence Panock

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-10-28 21:18
CPC Classifications
H; H10; H10P; H10P50/00; H10P50/69; C; C25; C25F; C25F3/00; C25F3/02; C25F3/12; H10P50/20; H10P50/60; H10P50/61; H10P50/617; H10P52/00; H10P95/00; H10P95/70

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 161 words
A process for fabricating a semiconductor device comprising at least one intrinsic or n-type compound semiconductor and having substantially damage-free surface, comprising the step of electrochemically etching at least a part of the surface of a compound semiconductor to produce oxidized species by passing current through the compound semiconductor, an electrolytic solution with conductivity greater than 0.0001 mhos/cm and a cathode, CHARACTERIZED BY conducting the etching as a photoetching procedure comprising applying a potential to the semiconducting compound which is between the maximum potential of the valence band of the semiconductor compound in the electrolytic solution and the minimum potential of the conduction band of the semiconductor compound in the electrolytic solution, illuminating that part of the surface of the compound semiconductor which is to be etched with radiation of sufficient energy to produce holes in the valence band, and including in the composition of the electrolytic solution species which removes the oxidized species from the surface of the compound semiconductor.
Claim 2
Dependent Claim 161 words
A process for fabricating a semiconductor device comprising at least one intrinsic or n-type compound semiconductor and having substantially damage-free surface, comprising the step of electrochemically etching at least a part of the surface of a compound semiconductor to produce oxidized species by passing current through the compound semiconductor, an electrolytic solution with conductivity greater than 0.0001 mhos/cm and a cathode, CHARACTERIZED BY conducting the etching as a photoetching procedure comprising applying a potential to the semiconducting compound which is between the maximum potential of the valence band of the semiconductor compound in the electrolytic solution and the minimum potential of the conduction band of the semiconductor compound in the electrolytic solution, illuminating that part of the surface of the compound semiconductor which is to be etched with radiation of sufficient energy to produce holes in the valence band, and including in the composition of the electrolytic solution species which removes the oxidized species from the surface of the compound semiconductor.
Claim 3
Dependent Claim 23 words
The process according to claim 1, CHARACTERIZED IN THAT the pH of the electrolytic solution is greater than 9, preferably greater than 11.
Claim 4
Dependent Claim 23 words
The process according to claim 1, CHARACTERIZED IN THAT the pH of the electrolytic solution is less than 5, preferably less than 3.
Claim 5
Dependent Claim 21 words
The process according to claim 3, CHARACTERIZED IN THAT the electrolytic solution comprises an acid selected from HF, HC1 and HBr.
Claim 6
Dependent Claim 25 words
The process according to claim 4, CHARACTERIZED IN THAT the acid concentration varies from about 0.05 to 10 molar, preferably between 0.2 and 2.0 molar.
Claim 7
Dependent Claim 42 words
The process according to claim 1, CHARACTERIZED IN THAT the compound is selected from III-V compound semiconductors such as GaP, GaAs, AlAs, AlP, AlSb, InSb, InAs, InP, GaInAs, GaInP, GaInAsP, GaAlP and GaAlAs, or II-VI compound semiconductors such as CdS, CdSe, HgCdTe,
Claim 8
Dependent Claim 31 words
The process according to claim 1, CHARACTERIZED IN THAT the compound semiconductor is n-type in which the doping level is between 10 15 and 10 19 atoms per cubic centimeter. -
Claim 9
Dependent Claim 42 words
The process according to claim 1 or 4 or 5, CHARACTERIZED IN THAT the compound is n-type InP and the potential of the SCE scale is between -0.5 and +1.0 volts, preferably between -0.1 and +0.5 volts in one molar hydrochloric acid.
Claim 10
Dependent Claim 43 words
The process according to claim 1 or 4 or 5, CHARACTERIZED IN THAT the compound semiconductor is n-type GaAs and the potential is between -0.7 and +1.0 volts, preferably between -0.4 and +0.4 volts, on the SCE scale in one molar hydrochloric acid.
Claim 11
Dependent Claim 24 words
The process according to claim 1, CHARACTERIZED IN THAT the energy of the radiation is greater than the band gap of the compound semiconductor.
Claim 12
Dependent Claim 80 words
The process according to claim 1, CHARACTERIZED IN THAT the device is a photodiode having an n-type' InP substrate, with a thin layer of n-type InP then a thin layer of n-type InGaAs and then a layer of p-type InGaAs, a hole is photoetched in the center of the photodiode structure n-type layer and intrinsic layer by electrochemical photoetching with a potential of 0.2 + 0.1 volts on the SCE scale and an electrolytic solution comprising one molar hydrochloric acid.
Claim 13
Dependent Claim 17 words
The process according to claim 11, CHARACTERIZED BY etching the p-type layer with a suitable chemical etch.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag