Abstract

Abstract A filled arylene sulfide polymer composition is provided in which at least 30 weight percent of the total composition is arylene sulfide polymer, up to about 65 weight percent of the total composition is filler material chosen from glass filler and at least one mineral filler and containing a property modifying amount of up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having the vinyl content in the range of about 10 to about 14 percent based on the polybutadiene segment of the copolymer. The physical characteristics of a filled arylene sulfide polymer composition containing at least 30 weight percent of the total composition of arylene sulfide polymer and up to about 65 weight percent of the total composition of fillers comprising glass fibers and at least one mineral filler are improved by the addition of a property modifying amount of up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having a vinyl content in the range of about 10 to about 14 percent based on the polybutadiene segment of the copolymer.

Inventors

  • 👤 Donald Gene Needham

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-11-02 13:54
CPC Classifications
C; C08; C08L; C08L81/00; C08L81/02; C08K; C08K3/00; C08K3/01; C08K3/013; C08K7/00; C08K7/02; C08K7/04; C08K7/14; C08L53/00; C08L53/02

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 81 words
A filled arylene sulfide composition comprising (a) at least 30 weight percent of the total composition of arylene sulfide polymer, (b) up to about 65 weight percent of the total composition of fillers comprising glass filler and at least one mineral filler and (c) up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having a vinyl content in a range of 10 to 14 percent based on the polybutadiene segment of the polymer.
Claim 2
Dependent Claim 81 words
A filled arylene sulfide composition comprising (a) at least 30 weight percent of the total composition of arylene sulfide polymer, (b) up to about 65 weight percent of the total composition of fillers comprising glass filler and at least one mineral filler and (c) up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having a vinyl content in a range of 10 to 14 percent based on the polybutadiene segment of the polymer.
Claim 3
Dependent Claim 22 words
The composition of claim 1 characterized in that said fillers (b) comprise from 55 to 65 weight percent of the total composition.
Claim 4
Dependent Claim 32 words
The composition of claim 1 or 2 characterized in that said fillers (b) comprise glass fiber and mineral filler in a ratio of 1:3 to 3:1 of glass filler to mineral filler.
Claim 5
Dependent Claim 26 words
The composition of any of claims 1 to 3 characterized in that said mineral filler is selected from calcium carbona-' te, calcium sulfate, talc, and mica.
Claim 6
Independent Claim 89 words
A method for improving physical characteristics of a filled arylene sulfide polymer composition containing at least 30 weight percent of the total composition of arylene sulfide polymer and up to about 65 weight percent of the total composition of fillers comprising glass fillers and at least one mineral filler,characterized by admixing therewith up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having a vinyl content in the range of 10 to 14 percent based on the polybutadiene segment of the copolymer.
Claim 7
Independent Claim 89 words
A method for improving physical characteristics of a filled arylene sulfide polymer composition containing at least 30 weight percent of the total composition of arylene sulfide polymer and up to about 65 weight percent of the total composition of fillers comprising glass fillers and at least one mineral filler,characterized by admixing therewith up to about 12 weight percent of the total composition of a solid, resinous butadiene/styrene block copolymer having a vinyl content in the range of 10 to 14 percent based on the polybutadiene segment of the copolymer.
Claim 8
Dependent Claim 19 words
The method of claim 5 characterized by utilizing fillers (b) in accordance with any of claims 2 to 4.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag