Process of producing optically anisotropic carbonaceous pitch

Assignee: Tonen General Sekiyu KK
•
Filing: 1982-01-27
•
Granted: —
•
Expires: 2002-01-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing a homogeneous, optically anisotropic carbonaceous pitch useful for the production of carbon materials, comprises the steps of thermally cracking and polycondensing a starting oil obtained from petroleum or coal, said starting oil comprising a substantially chloroform-insoluble matter-free oily or tarry substance including a mixture of compounds consisting mainly of carbon and hydrogen having a boiling point of main components in the approximate range 250 to 540 DEG C and containing n-heptane-soluble aromatic oil and resin as the main components, each of which has an aromatic carbon fraction of at least 0.6, preferably at least 0.7, a number-average molecular weight of up to 1000 and a maximum molecular weight of up to 2000.

Inventors

  • 👤 Takayuki Izumi
  • 👤 Tsutomu Naito
  • 👤 Tomoo Nakamura
  • 👤 Hisao Tanaka

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-11-09 06:44
CPC Classifications
D; D01; D01F; D01F9/00; D01F9/08; D01F9/12; D01F9/14; D01F9/145; D01F9/15; C; C10; C10C; C10C3/00; C10C3/002

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 116 words
A process for producing a homogeneous, optically anisotropic carbonaceous pitch useful for the production of carbon materials, characterized by the steps of thermally cracking and polycondensing a starting oil obtained from petroleum or coal, said starting oil comprising a substantially chloroform-insoluble matter-free oily or tarry substance including a mixture of compounds consisting mainly of carbon and hydrogen having a boiling point of main components in the approximate range of 250 to 540°C and containing n-heptane-soluble aromatic oil and resin as the main components, each of which has an aromatic carbon fraction of at least 0.6, preferably at least 0.7, a number-average molecular weight of up to 1000 and a maximum molecular weight of up to 2000.
Claim 2
Dependent Claim 116 words
A process for producing a homogeneous, optically anisotropic carbonaceous pitch useful for the production of carbon materials, characterized by the steps of thermally cracking and polycondensing a starting oil obtained from petroleum or coal, said starting oil comprising a substantially chloroform-insoluble matter-free oily or tarry substance including a mixture of compounds consisting mainly of carbon and hydrogen having a boiling point of main components in the approximate range of 250 to 540°C and containing n-heptane-soluble aromatic oil and resin as the main components, each of which has an aromatic carbon fraction of at least 0.6, preferably at least 0.7, a number-average molecular weight of up to 1000 and a maximum molecular weight of up to 2000.
Claim 3
Dependent Claim 37 words
A process according to claim 1, wherein the aromatic oil and resin have a number-average molecular weight of up to 750, preferably in the range 250 to 750, and a maximum molecular weight of up to 1,500.
Claim 4
Dependent Claim 28 words
A process according to claim 1 or claim 2, wherein the thermal cracking and polycondensation steps are carried out at a temperature in the range 380 to 460°C.
Claim 5
Dependent Claim 18 words
A process according to any preceding claim, wherein the starting oil further contains asphaltene as a n-heptane-insoluble component.
Claim 6
Dependent Claim 34 words
A process according to claim 4, wherein asphaltene has an aromatic carbon fraction of at least 0.6, a number-average molecular weight of up to 1000 and a maximum molecular weight of up to 2000.
Claim 7
Dependent Claim 23 words
A process according to claim 5, wherein the aromatic oil, resin and asphaltene each have an aromatic carbon fraction of at least 0.7.
Claim 8
Dependent Claim 40 words
A process according to any one of claims 4 to 6 wherein the aromatic oil, resin and asphaltene has a number-average molecular weight of up to 750, preferably 250 to 750, and a maximum molecular weight of up to 1500.
Claim 9
Dependent Claim 32 words
A process according to any preceding claim, wherein the optically anisotropic, carbonaceous pitch has a softening point in the approximate range of 230-320°C and an optically anisotropic phase content of approximately 90-100%.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag