Abstract

Abstract A developed composition for a lithographic printing plate provided with a coated layer composed of a photosensitive polymer having in the main chain thereof groups of formula (I) wherein X and Y independently represent hydrogen, halogen, cyano or nitro and n is an integer of 1 or 2, comprising: (A) benzyl alcohol, (B) tetrahydrofurfuryl alcohol and (C) at least one acid selected from the group consisting of a mineral acid, an organic carboxylic acid and an organic sulfonic acid.

Inventors

  • 👤 Shigeki Shimizu
  • 👤 Akinobu Oshima
  • 👤 Hiroshi Ide
  • 👤 Noriaki Takahashi

Bibliographic Details

Application Number —
Jurisdiction EP
Data Source google_patents
Last Synchronized 2026-11-01 22:46
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/26; G03F7/30; G03F7/32

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 39 words
A developer composition for a lithographic printing plate characterised in that it comprises: (A) benzyl alcohol, (B) tetrahydrofurfuryl alcohol and (C) at least one acid which is a mineral acid, an organic carboxylic acid or an organic sulfonic acid.
Claim 2
Dependent Claim 39 words
A developer composition for a lithographic printing plate characterised in that it comprises: (A) benzyl alcohol, (B) tetrahydrofurfuryl alcohol and (C) at least one acid which is a mineral acid, an organic carboxylic acid or an organic sulfonic acid.
Claim 3
Dependent Claim 30 words
A developer composition of claim 1, further characterised in that the amount of (A) benzyl alcohol in said developer composition is in the range of 5 to 90 wt. %.
Claim 4
Dependent Claim 23 words
A developer composition as claimed in claim 2 further characterised in that it comprises 30 to 70% by weight of (A) benzyl alcohol.
Claim 5
Dependent Claim 37 words
A developer composition as claimed in any one of claims 1 to 3 further characterised in that the amount of (B) tetrahydrofurfuryl alcohol in said developer composition is in the range of 5 to 90 wt. %.
Claim 6
Dependent Claim 23 words
A developer composition as claimed in claim 4 further characterised in that it comprises 10 to 40% by weight of (B) tetrahydrofurfuryl alcohol.
Claim 7
Dependent Claim 39 words
A developer composition as claimed in any one of claims 1 to 5, further characterised in that the amount of ( C ) the acid in said developer composition is in the range of 0.1 - 15 wt. %.
Claim 8
Dependent Claim 24 words
A developer composition as claimed in any one of claims 1 to 6 further characterised in that (C) the acid is a mineral acid.
Claim 9
Dependent Claim 18 words
A developer composition as claimed in claim 7, further characterised in that the mineral acid is phosphoric acid.
Claim 10
Independent Claim 107 words
A method of developing an image in a light exposed photosensitive coating of a lithographic printing plate, said coating composed of a photosensitive polymer having in the main chain thereof groups of the formula: wherein X and Y independently represent hydrogen, halogen, cyano or nitro, and n in an integer of one or two, comprising: washing the exposed portions of said exposed photosensitive coating from said plate with a developer solution and characterised in that the developer solution comprises: (A) benzyl alcohol, ( B ) tetrahydrofurfuryl alcohol and (C) at least one acid which is a mineral acid, an organic carboxylic acid or an organic sulfonic acid.
Claim 11
Independent Claim 107 words
A method of developing an image in a light exposed photosensitive coating of a lithographic printing plate, said coating composed of a photosensitive polymer having in the main chain thereof groups of the formula: wherein X and Y independently represent hydrogen, halogen, cyano or nitro, and n in an integer of one or two, comprising: washing the exposed portions of said exposed photosensitive coating from said plate with a developer solution and characterised in that the developer solution comprises: (A) benzyl alcohol, ( B ) tetrahydrofurfuryl alcohol and (C) at least one acid which is a mineral acid, an organic carboxylic acid or an organic sulfonic acid.
Claim 12
Dependent Claim 38 words
An image bearing developed lothographic printing plate characterised in that the plate has been developed using a developing composition as claimed in any one of claims 1 to 8 or by a method as claimed in claim 9.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Maintenance schedule is calculated for granted US utility patents.

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag