Water-soluble copolyesters, process for their preparation, and their use
Abstract
Abstract Copolyesters of the formula I <IMAGE> in which R is from 60 to 85 mol% of 1,3-phenylene radicals, from 5 to 20 mol% of tetramethylene radicals and from 10 to 20 mol% of, for example, radicals of the formula IIa <IMAGE> R<1> is from 60 to 95 mol% of ethylene radicals (-CH2CH2-), from 0 to 28 mol% of 2,2-dimethyl-1,3-propylene radicals and from 5 to 12 mol% of polyoxyethylene radicals having a mean molecular weight of up to 600, R<2> is, for example, SO3H, E and E<1> are, for example, -OH, and n is a number so large that the copolyester has a mean molecular weight of between 15000 and 40000, are used in the form of their aqueous solutions as sizing agents (sizes).
Inventors
- 👤 Friedrich Dipl.-Chem. Dr. Engelhardt
- 👤 Karl Dipl.-Chem. Dr. 6000 Frankfurt Hintermeier
- 👤 Rolf Dipl.-Chem. Dr. 6078 Neu-Isenburg Kleber
- 👤 Peter Dipl.-Chem. Dr. 6200 Wiesbaden Klein
Bibliographic Details
Claims Analysis
Total Claims: 0References Cited (Backward Citations)
No citation records indexed.
USPTO Annuity & Maintenance Windows
Maintenance schedule is calculated for granted US utility patents.